性能项目
|
试验条件[状态]
|
测试方法
|
测试数据
|
数据单位
|
|
基本性能
|
密度
|
ASTM D-1505
|
0.948
|
g/cm3
|
|
熔体流动速率
|
ASTM D-1238
|
4.0
|
g/10min
|
||
VA含量
|
26
|
%
|
|||
机械性能
|
硬度
|
ASTM D-2240
|
32
|
Shore D
|
|
拉力降伏强度
|
ASTM D-638
|
30
|
kg/cm2
|
||
弯曲模量
|
ASTM D-790
|
70
|
kg/cm2
|
||
硬度
|
ASTM D-2240
|
82
|
Shore A
|
||
拉力断裂强度
|
ASTM D-638
|
140
|
kg/cm2
|
||
拉力断裂伸长率
|
ASTM D-638
|
800
|
%
|
||
热性能
|
软化点
|
ASTM D-1525
|
48
|
℃
|
|
熔点
|
DSC
|
76
|
℃
|
||
脆化温度
|
ASTM D-746
|
<-70
|
℃
|
台塑EVA7470M